Reduction of wear via hardfacing of chisel ploughshare

dc.contributor.authorBayhan, Y
dc.date.accessioned2024-06-12T11:17:14Z
dc.date.available2024-06-12T11:17:14Z
dc.date.issued2006
dc.departmentTrakya Üniversitesien_US
dc.description.abstractThe objective of this study was to increase the wear resistance by covering the chisel ploughshare produced from low-alloy steel with three different hard facing electrodes. Comparative wear tests on a regular share and three kinds of hardfacing with electrodes were conducted in the field and laboratory. These three different hardfacing electrodes, which are designated EH-600, EH-350 and EH-14Mn, were used for hardfacing. The wear rate in the laboratory and in field tests was found to be significantly different statistically. When the cost is taken into consideration; EH-600 and EH-350 have been found to be the best hardfacing electrodes. (c) 2005 Elsevier Ltd. All rights reserved.en_US
dc.identifier.doi10.1016/j.triboint.2005.06.005
dc.identifier.endpage574en_US
dc.identifier.issn0301-679X
dc.identifier.issue6en_US
dc.identifier.scopus2-s2.0-31544438853en_US
dc.identifier.scopusqualityQ1en_US
dc.identifier.startpage570en_US
dc.identifier.urihttps://doi.org/10.1016/j.triboint.2005.06.005
dc.identifier.urihttps://hdl.handle.net/20.500.14551/24627
dc.identifier.volume39en_US
dc.identifier.wosWOS:000236397700016en_US
dc.identifier.wosqualityQ1en_US
dc.indekslendigikaynakWeb of Scienceen_US
dc.indekslendigikaynakScopusen_US
dc.language.isoenen_US
dc.publisherElsevier Sci Ltden_US
dc.relation.ispartofTribology Internationalen_US
dc.relation.publicationcategoryMakale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanıen_US
dc.rightsinfo:eu-repo/semantics/closedAccessen_US
dc.subjectWearen_US
dc.subjectTillage Toolsen_US
dc.subjectHardfacingen_US
dc.subjectCoatingsen_US
dc.titleReduction of wear via hardfacing of chisel ploughshareen_US